PlasmaforumPLASMA SURFACE TECHNIQUE |
![]() |
Posted by Aranguren on August 28, 2003 at 08:44:43:
In Reply to: Re: White Layer posted by David on August 27, 2003 at 14:31:24:
Thanks a lot, David.
The Gear is used in a multiplier, so the dynamic loads are important. I think that the best solution would be Plasma-Nitriding. But, isnīt it more expensive?
See you